Dental glass ceramics, Main ingredients are Lithium Disilicate, through special process. HT--High Transparency. HT-- A1, A2, A3,B1,B2, BL1, BL2, BL3, BL4,C1,C2. Bending strength The average biaxial bending strength after being fully crystallized is 637Mpa, higher than the standard strength value, set by ISO6892:2008 For Dental Ceramics.
| Pack | 1 Box (5Pcs/Box) |
| Brand | Pinlide |
| System: | CAD/CAM |
| Type | C14 |
| Size | 18*15*13mm |
| Country/Region Of Manufacture | China |
| C14 HT/LT | High Transparency |
| Country Of Origin | China |
Dental glass ceramics, Main ingredients are Lithium Disilicate, through special process. HT–High Transparency. HT– A1, A2, A3,B1,B2, BL1, BL2, BL3, BL4,C1,C2. Bending strength The average biaxial bending strength after being fully crystallized is 637Mpa, higher than the standard strength value, set by ISO6892:2008 For Dental Ceramics.